Basic Info.
Alkali Content
Alkali Free
Area Weight
18oz(600GSM)
Roll Width
1250mm
Moisture Content %
≤0.1
Loss of Ignition
0.4-0.8%
Transport Package
in Carton Box
Specification
18oz (600gsm)
Trademark
JLON
Origin
China
HS Code
70194000
Production Capacity
20000ton
Product Description
If you search for Hand Lay-up products, we can provide not only chop strand mat, but also woven roving, you can read below related products for reference.
Woven roving
Introduction:
Fiberglass Woven Roving is bidirectional fabric made by interweaving direct roving. Can be compatible with unsaturated polyester, vinyl ester, epoxy and phenolic resins. With high-performance reinforcement, widely used in hand lay up to manufacture boats, vessels, plane and automotive parts, furniture and sports facilities. The area weight is from 200g/m2 to 1200g/m2. The width is from 50mm-3000mm.
Specifications:
Related Product-Chopped Strand Mat(Suitable for Hand Lay-up)
Chopped strand mat is produced by chopping continuous roving into length of 5cm and randomly dispersing the cut fibers. These fibers are held together by powder or emulsion binder. It is typically used for hand lay up process. The mats are compatible with unsaturated polyester, vinyl ester and PU resins. Width ranges from 50mm to 3200mm.
Application: panels, tanks, boats, complete set of sanitary equipment, automotive parts, cooling towers, pipes etc
Specifications:
Woven roving
Introduction:
Fiberglass Woven Roving is bidirectional fabric made by interweaving direct roving. Can be compatible with unsaturated polyester, vinyl ester, epoxy and phenolic resins. With high-performance reinforcement, widely used in hand lay up to manufacture boats, vessels, plane and automotive parts, furniture and sports facilities. The area weight is from 200g/m2 to 1200g/m2. The width is from 50mm-3000mm.
Specifications:
Product No. | Glass | Weight(g/m²) | Breaking Strength ≥N/25MM | Weave | Moisture Content % | L.O.I Content % | |
Warp | Weft | ||||||
WR200 | E | 200+/-10 | 820 | 700 | Plain | ≤0.1 | 0.4-0.8 |
WR270 | E/ECR | 270+/-14 | 1200 | 1000 | Plain | ≤0.1 | 0.4-0.8 |
WR300 | E | 300+/-15 | 1200 | 1200 | Plain | ≤0.1 | 0.4-0.8 |
WR360 | E/ECR | 400+/-20 | 1200 | 1150 | Plain | ≤0.1 | 0.4-0.8 |
WR400 | E | 400+/-20 | 1480 | 1380 | Plain | ≤0.1 | 0.4-0.8 |
WR500T | E | 500+/-25 | 1800 | 1700 | Twill | ≤0.1 | 0.4-0.8 |
WR500 | E | 500+/-25 | 1800 | 1600 | Plain | ≤0.1 | 0.4-0.8 |
WUDT500 | E | 500+/-25 | 100 | 2900 | Plain | ≤0.1 | 0.4-0.8 |
WUDL500 | E | 500+/-25 | 2600 | 350 | Plain | ≤0.1 | 0.4-0.8 |
WUDL530 | E | 530+/-27 | 3200 | 800 | Plain | ≤0.1 | 0.4-0.8 |
WR580 | E/ECR | 580+/-29 | 1900 | 1600 | Plain | ≤0.1 | 0.4-0.8 |
WR600 | E | 600+/-30 | 1900 | 1800 | Plain | ≤0.1 | 0.4-.8 |
WR600B | E | 600+/-30 | 1900 | 1850 | Plain | ≤0.1 | 0.4-0.8 |
WUDL600 | E | 600+/-30 | 3100 | 350 | Plain | ≤0.1 | 0.4-0.8 |
WR800 | E | 800+/-40 | 2600 | 2300 | Plain | ≤0.1 | 0.4-0.8 |
WR800A | E | 864+/-43 | 2900 | 2700 | Plain | ≤0.1 | 0.4-0.8 |
WR1000 | E | 1000+/-50 | 2900 | 2900 | Plain | ≤0.1 | 0.4-0.8 |
Related Product-Chopped Strand Mat(Suitable for Hand Lay-up)
Chopped strand mat is produced by chopping continuous roving into length of 5cm and randomly dispersing the cut fibers. These fibers are held together by powder or emulsion binder. It is typically used for hand lay up process. The mats are compatible with unsaturated polyester, vinyl ester and PU resins. Width ranges from 50mm to 3200mm.
Application: panels, tanks, boats, complete set of sanitary equipment, automotive parts, cooling towers, pipes etc
Specifications:
Item | Weight(g/m2) | Binder Content(%) | Water Content(%) |
EMC100 | 100 | 9-12 | <0.2 (powder bonded) <0.5 (emulsion bonded) |
EMC150 | 150 | 9-12 | <0.2 (powder bonded) <0.5 (emulsion bonded) |
EMC225 | 225 | 2-8 | <0.2 (powder bonded) <0.5 (emulsion bonded) |
EMC300 | 300 | 2-8 | <0.2 (powder bonded) <0.5 (emulsion bonded) |
EMC450 | 450 | 2-8 | <0.2 (powder bonded) <0.5 (emulsion bonded) |
EMC600 | 600 | 2-8 | <0.2 (powder bonded) <0.5 (emulsion bonded) |